特征 Features
直径1-5mm的聚四氟乙烯挤出棒是选用聚四氟乙烯树脂经糊膏挤压加工成;直径6-200mm的棒选用悬浮聚四氟乙烯树脂经柱塞加工制成直径200mm以上的棒经模压加工制成。
Diameter 1-5mm rods are made of polytetraflu resin by paste extrusion processing: Diameter 6-200mm rod selection suspension PTFE resin made by plunger processing Diameter more than 200mm rods by molding production
型号及规格 Types and Specifications
注:当棒直径大于16mm时,仅测试表观密度
Note: When the diameter of rod is larger than 1 6mm, only test apparent density
主要技术指标 Main Properties:
用途App| ications
化工方面:能用作防腐资料,可制造各种防腐蚀零部件,如管子、阀门、泵及管件接头等。化工设备方面,可制作反应器、蒸馏塔及防腐设备的衬里和涂层。机械方面:可用作自润滑轴承、活塞环、油封及密封圈等。自润滑性可减少机件磨损和发热,降低动力消耗。电子电器方面:主要用于制造各种电线电缆、电池电极、电池隔膜、印刷电路板等。
Chemical: can be used as anti-corrosion materials, can manufacture a variety of anti-corrosion parts, su
as pipes, valves, pumps and fittings joints. Chemical equipment, can be produced reactor, distillation column
anti-corrosion equipment lining and coating
Mechanical: can be used as self-lubricating bearings, piston rings oil seals and seals. Self-lubrication can
duce wear and heat and reduce power consur
Electronic and electric
pects:mainly used in the manufacture of various wire and cable, battery elec
trodes, battery separator, printed circuit boards
本文由聚四氟乙烯挤出棒生产厂家扬中市亚达橡塑制品有限公司于2018/11/8 17:30:50整理发布。
上一篇:没有了!
下一篇:聚四氟乙烯模压棒
2018受供给侧改革、环保督察的影响,从上游原材料到中游氢氟酸到下游氟树脂行业,厂家整体开工率不高,产品供应紧张,市场仍会处于供不应求状态,产量收缩,价格预计继续上涨。
发布时间:2018-11-12我们工程都是根据HG2099来检测聚四氟乙烯密封垫片的 “走漏量”,单端面的机械密封只是针对“走漏量”做定性检查,我们肉眼看不到显著气泡就算合格。一般我们检测的规则是轴径≥80mm时,走漏量是≤10L/h的;轴径≤80mm时,走漏量是≤8mL/h的。
发布时间:2018-11-12聚四氟乙烯垫片失效后会产生泄漏,主要表现在一是密封面上有间隙。二是密封部位两侧存在压力差。聚四氟乙烯垫片密封需要解决的是消除或减小密封面之间的间隙。